Recommendation: |
the content of alloying element has little effect on the hardness of products,but the content of chromium and molybdenum |
has a big impact on products'actual abrasion resistance. |
Advantages: |
100% produced by us to control the production process strictly. |
100% delivery on time,deduct 1% of the total payment for one day delay and so on. |
Insure that inventory sales for the commonly used products to shorten the delivery time and increase the market |
competitiveness of customers. |
Part Number | A | B | C | D | E | Weight kg |
DLP 4 | 300 | 38 | 25 | 8 | 33 | 3 |
DLP 295 | 153 | 38 | 25 | 8 | 33 | 1.6 |
DLP 508 | 190 | 50 | 20 | 10 | 30 | 2.3 |
DLP 125 | 230 | 50 | 38 | 12 | 50 | 4.6 |
DLP 1101 | 150 | 50 | 40 | 10 | 50 | 3 |
DLP 528 | 150 | 75 | 40 | 10 | 50 | 4.5 |
DLP 619 | 150 | 75 | 50 | 10 | 60 | 5.3 |